Information provided by Vyncolit, a Sumitomo Bakelite Group
| 物理性能 | 额定值 (公制) | 额定值 (英制) | 测试方法 |
|---|---|---|---|
| 体积密度 | g/cc | lb/in³ | Powder Density; ASTM D1895 |
| 密度 | g/cc | lb/in³ | Relative Density; ASTM D792 |
| 线性成型收缩率 | cm/cm | in/in | Compression Molding; ASTM D955 |
| 机械性能 | 额定值 (公制) | 额定值 (英制) | 测试方法 |
|---|---|---|---|
| 抗张强度(断裂) | MPa | psi | ASTM D638 |
| 弯曲强度 | MPa | psi | At Rupture; ASTM D790 |
| 弯曲模量 | GPa | ksi | ASTM D790 |
| 抗压强度 | MPa | psi | ASTM D695 |
| 悬壁梁缺口冲击强度 | J/cm | ft-lb/in | ASTM D256 |
| 电气性能 | 额定值 (公制) | 额定值 (英制) | 测试方法 |
|---|---|---|---|
| 介电常数 | @Frequency 1e+6 Hz | @Frequency 1e+6 Hz | Dry; ASTM D150 |
| 介电强度 | kV/mm | kV/in | 60Hz, Short Time, dry; ASTM D149 |
| 耗散因数 | @Frequency 1e+6 Hz | @Frequency 1e+6 Hz | Dry; ASTM D150 |
| 耐电弧性 | sec | sec | ASTM D495 |
| 热性能 | 额定值 (公制) | 额定值 (英制) | 测试方法 |
|---|---|---|---|
| 线形热膨胀系数 - 流动 | µm/m-°C @Temperature 20.0 °C | µin/in-°F @Temperature 68.0 °F | ASTM E-831 |
| 载荷下热变形温度(1.8 MPa) | >= °C | >= °F | Post Baked; ASTM D648A |
| 材料描述 | 测试方法 | |
|---|---|---|
| 颜色 | Black | |
| 形式 | Granular | |
| Main Filler | Glass Fiber & Mineral | |
| Molding Method | Compression, transfer |