登录

Styron INSPIRE™ TF3800 Polypropylene

Polypropylene (PP)

Styron

产品说明

Information provided by Dow

The Inspire brand was spun off from Dow Chemical to Styron in 2010

物理性能额定值 (公制)额定值 (英制)测试方法
比重 g/cc g/cc ASTM D792
熔体流动速率 g/10 min
@Load 2.16 kg, Temperature 230 °C
g/10 min
@Load 4.76 lb, Temperature 446 °F
ASTM D1238
机械性能额定值 (公制)额定值 (英制)测试方法
极限抗拉强度 MPa psi ASTM D638
抗张强度(屈服) MPa psi ASTM D638
伸长率 (断裂) ASTM D638
屈服伸长率 ASTM D638
拉伸模量 GPa ksi ASTM D638
弯曲强度 MPa psi ASTM D790
弯曲模量 GPa ksi ASTM D790
悬壁梁缺口冲击强度 J/cm
@Thickness 3.17 mm, Temperature -28.9 °C
ft-lb/in
@Thickness 0.125 in, Temperature -20.0 °F
ASTM D256
J/cm
@Thickness 3.17 mm, Temperature -17.8 °C
ft-lb/in
@Thickness 0.125 in, Temperature 0.000 °F
ASTM D256
J/cm
@Thickness 3.17 mm, Temperature 22.8 °C
ft-lb/in
@Thickness 0.125 in, Temperature 73.0 °F
ASTM D256
Dart Drop, Total Energy J
@Temperature 22.8 °C
ft-lb
@Temperature 73.0 °F
ASTM D3763
J
@Temperature -17.8 °C
ft-lb
@Temperature 0.000 °F
ASTM D3763
J
@Temperature -28.9 °C
ft-lb
@Temperature -20.0 °F
ASTM D3763
J
@Temperature -33.9 °C
ft-lb
@Temperature -29.0 °F
ASTM D3763
Falling Dart Impact J ft-lb 73°F, Peak Energy; ASTM D3763
J ft-lb 0°F, Peak Energy; ASTM D3763
J ft-lb -20°F, Peak Energy; ASTM D3763
J ft-lb -29°F, Peak Energy; ASTM D3763
热性能额定值 (公制)额定值 (英制)测试方法
线性热膨胀系数 µm/m-°C
@Temperature -30.0 - 30.0 °C
µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
载荷下热变形温度(0.46 MPa) °C
@Thickness 3.17 mm
°F
@Thickness 0.125 in
Unannealed; ISO 75-2-92
载荷下热变形温度(1.8 MPa) °C
@Thickness 3.17 mm
°F
@Thickness 0.125 in
Unannealed; ISO 75-2-92
Copyright © souwuxing.com All Rights Reserved. 归 搜聚信息科技公司 所有
此数据表中的信息由 搜聚 从该材料的生产商处获得。搜聚 尽最大努力确保此数据的准确性。 但是 搜聚 对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。