登录

Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data)

High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight

Quadrant Engineering Plastics Products

产品说明

TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufacturing paper with high abrasive filler content.

物理性能额定值 (公制)额定值 (英制)测试方法
密度 g/cc lb/in³ ISO 1183-1
吸水率 96 hr; ISO 62
平衡吸湿 50% RH
饱和吸水率 ISO 62
Outgassing - Total Mass Loss
机械性能额定值 (公制)额定值 (英制)测试方法
肖氏硬度 (邵氏 D)
球压硬度 MPa psi ISO 2039-1
抗张强度 MPa psi at Yield; ISO 527-1/-2
伸长率 (断裂) ISO 527-1/-2
屈服伸长率 ISO 527-1/-2
拉伸模量 GPa ksi ISO 527-1/-2
弯曲强度 MPa psi
抗压强度 MPa
@Strain 1 %
psi
@Strain 1 %
ISO 604
MPa
@Strain 2 %
psi
@Strain 2 %
ISO 604
MPa
@Strain 5 %
psi
@Strain 5 %
ISO 604
K Factor (ISO) µm/km µm/km
简支梁无缺口冲击强度 ISO 179-1/1eU
简支梁缺口冲击强度 J/cm² ft-lb/in² Partial Break; ISO 179-1/1eA
动态摩擦系数
Sand Slurry
Limiting Pressure Velocity MPa-m/sec psi-ft/min at 1 m/s unlubricated
MPa-m/sec psi-ft/min at 0.1 m/s unlubricated
电气性能额定值 (公制)额定值 (英制)测试方法
体积电阻率>= ohm-cm >= ohm-cm IEC 60093
表面电阻率>= ohm >= ohm IEC 60093
介电强度 kV/mm kV/in
热性能额定值 (公制)额定值 (英制)测试方法
线性热膨胀系数 µm/m-°C
@Temperature 23.0 - 100 °C
µin/in-°F
@Temperature 73.4 - 212 °F
导热系数 W/m-K BTU-in/hr-ft²-°F
熔融温度 °C °F DSC, 10°C/min.; ISO 11357-1/-3
最高工作温度, Air °C °F Continuous
载荷下热变形温度(1.8 MPa) °C °F ISO 75-1/-2
可燃性(UL94)
极限氧指数 ISO 4589-1/-2
合规性额定值 (公制)额定值 (英制)测试方法
3A-Dairy
European Food 1935/2004
FDA
USP Class VI
耐化学性能额定值 (公制)额定值 (英制)测试方法
Acids, Strong (pH 1-3)
Acids, Weak
Alcohols
Alkalies, Strong (pH 11-14)
Alkalies, Weak
Chlorinated Solvents
Continuous Sunlight
Hot Water / Steam
Hydrocarbons - Aliphatic
Hydrocarbons - Aromatic
Inorganic Salt Solutions
Ketones, Esters
Copyright © souwuxing.com All Rights Reserved. 归 搜聚信息科技公司 所有
此数据表中的信息由 搜聚 从该材料的生产商处获得。搜聚 尽最大努力确保此数据的准确性。 但是 搜聚 对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。
微信小程序 搜物性手机端