登录

TOTAL Polyethylene Lumicene® M 3410 EP (EU)

MDPE

TOTAL Refining & Chemicals

产品说明

Lumicene® mPE M 3410 EP is a second generation metallocene based Medium Density Polyethylene with hexene as comonomer.

Lumicene® mPE M 3410 EP can be processed at high output rates with low extrusion pressure, excellent bubble stability and gauge control in comparison with conventional LLDPE and first generation metallocene based polyethylene. The combination of these features brings a significant downgauging potential.

Lumicene® mPE M 3410 EP is especially dedicated to film applications where high gloss and high transparency are required, particularly in blend and in coextrusion with LLDPE or LDPE.

Lumicene® mPE M 3410 EP is suited for many applications in the field of consumer, industrial, food or hygiene packaging such as collation shrink, mailing film, heavy-duty sacks, bags, lamination and hygiene film.
基本信息
添加剂
  • 加工助剂
  • 抗氧化性
特性
  • 刚性,高
  • 高光
  • 己烯共聚单体
  • 抗穿孔性
  • 可热封
  • 良好的热封性
  • 良好的撕裂强度
  • 清晰度,高
用途
  • 包装
  • 薄膜
  • 层压板
  • 袋子
  • 多层薄膜
  • 混合
  • 食品包装
  • 收缩性薄膜
  • 消费品应用领域
  • 重包装袋
机构评级
  • EC 1907/2006 (REACH)
形式
  • 粒子
加工方法
  • 吹塑薄膜
  • 共挤出成型
物理性能额定值单位制测试方法
比重 g/cm³ASTM D792, ISO 1183
熔流率(熔体流动速率)
    190°C/2.16 kg g/10 minASTM D1238, ISO 1133
    190°C/21.6 kg g/10 minASTM D1238
机械性能额定值单位制测试方法
摩擦系数 (与自身 - 静态, 吹塑薄膜)ASTM D1894
薄膜额定值单位制测试方法
薄膜厚度 - 经测试 µm
割线模量 ASTM D882A
    1% 正割, MD : 吹塑薄膜 MPaASTM D882A
    1% 正割, TD : 25 µm, 吹塑薄膜 MPaASTM D882A
拉伸应力
    MD : 屈服, 40 µm, 吹塑薄膜 MPaISO 527-3
    TD : 屈服, 40 µm, 吹塑薄膜 MPaISO 527-3
    MD : 断裂, 25 µm, 吹塑薄膜 MPaASTM D882A
    TD : 断裂, 25 µm, 吹塑薄膜 MPaASTM D882A
    MD : 断裂, 40 µm, 吹塑薄膜 MPaISO 527-3
    TD : 断裂, 40 µm, 吹塑薄膜 MPaISO 527-3
伸长率
    MD : 断裂, 25 µm, 吹塑薄膜 %ASTM D882A
    TD : 断裂, 25 µm, 吹塑薄膜 %ASTM D882A
    MD : 断裂, 40 µm, 吹塑薄膜 %ISO 527-3
    TD : 断裂, 40 µm, 吹塑薄膜 %ISO 527-3
落锤冲击
    25 µm, 吹塑薄膜 gASTM D1709A
    40 µm, 吹塑薄膜 gISO 7765-1
埃尔曼多夫抗撕强度 ASTM D1922
    MD : 25 µm, 吹塑薄膜 gASTM D1922
    TD : 25 µm, 吹塑薄膜 gASTM D1922
始封温度 °C
水蒸气透过性 g/m²/24 hrASTM E96
Elmendorf Tear Strength 1ISO 6383-2
    MD : 40.0 µm kN/mISO 6383-2
    TD : 40.0 µm kN/mISO 6383-2
热性能额定值单位制测试方法
维卡软化温度 °CISO 306
熔融温度 °CISO 11357-3, ASTM D3417
光学性能额定值单位制测试方法
Gardner光泽度 (45°, 25.4 µm, 吹塑薄膜)ASTM D523
光泽度 (45°, 40.0 µm, 吹塑薄膜)ASTM D2457
雾度
    25.4 µm, 吹塑薄膜 %ASTM D1003
    40.0 µm, 吹塑薄膜 %ISO 14782
挤出额定值单位制
熔体温度 °C
备注
1 .Blown Film
Copyright © souwuxing.com All Rights Reserved. 归 搜聚信息科技公司 所有
此数据表中的信息由 搜聚 从该材料的生产商处获得。搜聚 尽最大努力确保此数据的准确性。 但是 搜聚 对这些数据值不承担任何责任,并强烈建议在最终选择材料前,就数据值与材料供应商进行验证。
微信小程序 搜物性手机端